Incoloy 864 Nickel Alloy Pipe (UNS S35135)
Incoloy 864 alloy pipe (UNS S35135) was specifically developed for automotive exhaust system flexible couplings, EGR tubes, manifolds and tailpipes. It exhibits excellent fatigue resistance, thermal stability and resistance to hot salt corrosion, pitting and chloride stress-corrosion cracking.
|
|
|
|
30 - 38 |
|
|
29.105 - 45 |
|
|
20 - 25 |
|
|
4 - 4.8 |
|
|
0.60 - 1 |
|
|
0.40 - 1 |
|
|
<= 0.080 |
|
|
<= 0.015 |
|
|
|
|
|
8.02 g/cm3 |
0.290 lb/in3 |
|
|
1353-1393℃ |
2467-2539℃F |
|
|
|
|
|
648 MPa |
94000 psi |
|
|
109.6 MPa |
15900 psi |
|
|
16.60% |
16.60% |
|
|
|
|
|
Thermal expansion co-efficient (@100℃/212℃F) |
14.7 µm/m℃ |
8.17 µin/in℃F |
|
Thermal conductivity (@23℃/73.4℃F) |
11 W/mK |
76.3 BTU.in/hrft².℃F |